How to Get Rid of Weeds Between Pavers for Good
10 mins read

How to Get Rid of Weeds Between Pavers for Good

Stopping weeds between pavers for good starts with removing the weeds and any old, failing joint sand down to the full joint depth, then reinstalling polymeric sand correctly: full depth, a dry surface, and a multi-pass misting activation. Pulling weeds without replacing the sand underneath just gives the next seed a wide-open joint to grow in.

Key takeaways

  • Weeds in paver joints are usually a symptom of sand that’s already failing, washed out, or never fully cured — not a standalone problem you can spray your way out of.
  • Polymeric sand has a minimum install depth (1.25-1.5 inches, depending on joint width) and sits about 1/8 inch below the paver surface, per two independent manufacturers’ data sheets.
  • The activation step — misting in several passes, not one quick spray — is what makes the sand harden enough to resist weeds and washout. Rushing it is the most common reason reinstalled sand fails again.
  • Manufacturers describe polymeric sand and sealers as reducing weed and ant problems, not eliminating them permanently — match your expectations to that, and keep an eye on joints over time.
  • If the joints you’re refilling sit next to a sunken or settled section, fix that first; see our guide to fixing sunken or uneven pavers.

Why do weeds keep coming back in the same joints?

The Interlocking Concrete Pavement Institute’s own technical guidance ties weed growth directly to joint sand condition: “Like sealers, joint and stabilization materials reduce the potential for weeds and ants in the joints.” Read that the other way around, and it says something useful — joints where the sand has washed out, cracked, or never properly cured are the joints where weeds take hold. A paver surface with intact, hardened polymeric sand in every joint gives a windblown seed nowhere to root.

That’s also why spraying the visible weed and moving on rarely works for long. If the sand underneath is still failing, you’ve removed the plant but not the opening it grew through.

A weed with green and reddish leaves growing up through the joint between two gray paving stones

Step 1: Remove the weed and the old sand around it

  1. Pull the weed, roots included. A paver joint weeding tool or a flathead screwdriver works for getting under the root without damaging the paver edge.
  2. Dig out the failing sand around it. Don’t just top off a joint that’s half-empty — remove old, degraded sand down to the paver’s full depth in that joint so the new sand has a clean, consistent base. Mixing old and new polymeric sand in the same joint can leave weak spots.
  3. Clear every joint you’re treating, not just the worst-looking ones. Joints right next to a weedy one are often just as compromised, even if nothing is growing there yet.
  4. Rinse and let the whole area dry completely before refilling. This matters more than it sounds — see the dry-surface requirement below.

Step 2: Reinstall polymeric sand to the right depth

This is the step most DIY weed-removal guides skip, and it’s the one that actually determines whether the fix lasts. SEK-Surebond’s Techo-Bloc PolySweep technical data sheet specifies a minimum joint depth of 1.5 inches for regular joints and 1.25 inches for X-Treme Wide Joint applications. Unilock’s own polymeric sand guidance corroborates the finish detail: joints should be filled to roughly 1/8 inch below the paver’s rounded or beveled edge — not flush with the surface, and not overfilled.

Spec Regular joint X-Treme Wide Joint Source
Minimum sand depth 1.5 in. 1.25 in. SEK-Surebond/Techo-Bloc PolySweep TDS
Fill level vs. paver edge About 1/8 in. below the chamfer/bevel, not flush PolySweep TDS; corroborated by Unilock’s own polymeric sand page
Surface condition required Completely dry; wet sand sticks to the paver face and is hard to remove PolySweep TDS
Weather window No rain forecast for 12+ hours; air temp above 35°F for 48+ hours after install PolySweep TDS

Exact minimum depths vary slightly by brand and joint width, so check your specific product’s data sheet if you’re not using PolySweep — but the principle holds across manufacturers: shallow, underfilled joints are weaker and fail faster.

A person wearing work gloves kneeling to set a paver into fresh sand next to other pavers, with sand and a trowel nearby
Removing old sand down to the full joint depth before refilling gives the new polymeric sand a clean, consistent base.

Step 3: Activate the sand correctly (this is where most DIY jobs fail)

Polymeric sand doesn’t harden on its own — it needs a specific water-activation sequence, and rushing it is the single most common reason reinstalled sand fails again within a season. PolySweep’s technical data sheet lays out the process:

  1. Distribute and sweep. Spread the sand evenly and sweep it into the joints until they’re full to the depth in the table above.
  2. Compact. Run a vibratory plate compactor over the area to settle the sand into the joints.
  3. Remove excess dust. Blow off any residual loose sand or dust with a leaf blower held nearly parallel to the surface — this prevents haze from unactivated sand drying on the paver face.
  4. First misting pass. Mist with a garden hose on a shower setting, no more than 500 square feet at a time, and let the water absorb for about 5 minutes.
  5. Repeat 3-4 times. Each pass uses a bit more water than the last, until the full joint depth is saturated. The final pass should rinse any remaining residue off the paver surface.
  6. Let it cure. Initial “set up,” strong enough to resist wind and light rain, happens within hours. A full hard cure depends on temperature and humidity and can take up to 24 hours or longer in cool, damp, or overcast conditions. PolySweep specifically reaches strong cohesion within about 12 hours of activation under normal conditions, per its own data sheet.
Original diagram showing polymeric sand joint depth specifications and a five-step activation and cure timeline: fill and sweep, compact, first misting, repeat misting, and cure
Original graphic: polymeric sand depth specs and the misting/cure timeline, from PolySweep and Unilock technical data sheets.

Does sealing the pavers help keep weeds out too?

Yes, according to the same ICPI guidance that connects joint sand to weed control: “Like stabilizers, sealers are also useful in stopping unwanted insects and weeds.” A sealed surface and solid joint sand work together — the sand physically fills the gap, and a sealer helps keep it from washing out as quickly. If your pavers haven’t been sealed yet, or it’s been a few years, see our complete guide to sealing pavers for the full process, including timing after a polymeric sand install.

Safety note: if you do seal after reinstalling sand, work in a ventilated outdoor area and wear the gloves and eye protection the sealer’s label recommends. Solvent-based sealers in particular give off strong fumes and should never be applied in an enclosed or poorly ventilated space, per manufacturer and ICPI safety guidance.

Several dandelions with yellow flowers growing in the joints between paving stones
Dandelions and other weeds root wherever joint sand has washed out or never fully cured — not randomly across a paver surface.

Will this stop weeds permanently?

Be realistic about what the products themselves claim. Neither ICPI nor the polymeric sand manufacturers we checked say joint sand or sealer eliminates weeds permanently — the language used is “reduce,” “lessen,” and “deter.” A properly reinstalled joint at full depth, correctly activated, is dramatically more weed-resistant than a shallow or half-cured one, but no paver joint is literally weed-proof forever. Spot-check joints once or twice a year, especially after a hard winter or heavy rain season, and address any sand that’s visibly eroding before a weed shows up in it.

Frequently asked questions

Can I just pull the weeds and leave the old sand?

You can, but expect the weed to come back. If the sand around it has already washed out or failed, the opening that let the weed root is still there. Removing the old sand down to full depth and reinstalling it correctly is what actually closes that opening.

How deep does polymeric sand need to be in the joints?

At least 1.5 inches for a regular joint, or 1.25 inches for an extra-wide joint, based on SEK-Surebond’s PolySweep technical data sheet. Check your specific product’s data sheet, since minimums vary slightly by brand and joint width.

Why did my polymeric sand fail or wash out after I installed it?

The most common cause is skipping or rushing the misting/activation step. Polymeric sand needs several misting passes over roughly 5-minute intervals to saturate the full joint depth, not one quick spray. Installing on a damp surface, or rain hitting the joints before the minimum cure window, can also cause early failure.

Do polymeric sand and sealer really stop ants too?

They reduce the risk, according to ICPI’s technical guidance, which lists ant and weed control together as a benefit of intact joint sand and sealer. Neither is described as a guaranteed, permanent fix for either problem.

How long do I need to wait before walking on newly reinstalled joints?

Initial set-up that resists wind and light rain happens within a few hours. For a full cure, plan on up to 24 hours or longer in cool, damp, or overcast weather before regular foot traffic, per PolySweep’s technical data sheet.

Sources

paversealguide.com Editorial Team. Last updated: November 13, 2026.

Leave a Reply

Your email address will not be published. Required fields are marked *